I need to do dissimilar weld joint (6xxx series Aluminium to Steel). What filler wire should I choose?

63 views
Skip to first unread message

Ram

unread,
May 23, 2019, 7:44:48 AM5/23/19
to Materials & Welding
I need to do dissimilar weld joint (6xxx series Aluminium to Steel). What filler wire should I choose?

PREM SHANKARDUTT NAUTIYAL

unread,
May 24, 2019, 2:26:14 AM5/24/19
to materials_welding
You cannot weld aluminum to steel by arc welding..


Regards

Prem Nautiyal


PREM S NAUTIYAL
CELL : 9769316004
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https:roups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7206cf51-d3f4-413a...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Karthik

unread,
May 24, 2019, 2:26:16 AM5/24/19
to Materials & Welding
Hi,
The attached file might be useful to you.

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282

E-mail : karthi...@yahoo.com



On Thursday, May 23, 2019, 6:44:48 PM GMT+7, Ram <rames...@gmail.com> wrote:


I need to do dissimilar weld joint (6xxx series Aluminium to Steel). What filler wire should I choose?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Aluminium Welding - pocket-guide.pdf

PGoswami

unread,
May 24, 2019, 11:56:27 PM5/24/19
to material...@googlegroups.com

Aluminum can’t be directly welded to Steel by any Arc welding process. Arc welding between any steel to aluminum causes formation of intermetallic compounds at the interface, which makes the weld joint extremely brittle. Look at the YouTube, there’re many videos on this subject.

 

The only way to perform arc welding of such dissimilar combination is to use a transition piece  of steel to Aluminum, produced by solid state welding process.

This article from ESAB , explains some of the problems of such welding.

 

Thanks.

P.Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@quickclic.net,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

 

From: 'Karthik' via Materials & Welding [mailto:material...@googlegroups.com]

Sent: May 23, 2019 10:07 PM
To: Materials & Welding <material...@googlegroups.com>

Subject: Re: [MW:29631] I need to do dissimilar weld joint (6xxx series Aluminium to Steel). What filler wire should I choose?

Hi,

The attached file might be useful to you.

 

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager

Agon Pacific Co.,Ltd.

M: +66-655-174-397, +66-892-512-282

 

 

On Thursday, May 23, 2019, 6:44:48 PM GMT+7, Ram <rames...@gmail.com> wrote:

 

 

I need to do dissimilar weld joint (6xxx series Aluminium to Steel). What filler wire should I choose?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7206cf51-d3f4-413a-838e-3036e9ad1a26%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.

Can I Weld Aluminum to Steel.pdf

Kannayeram Gnanapandithan

unread,
May 25, 2019, 1:44:06 AM5/25/19
to materials-welding
Direct fusion welding not possible
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


Karthik

unread,
May 25, 2019, 1:44:06 AM5/25/19
to Materials & Welding
Hi,
Please find the below link from ESAB regarding welding of Aluminum to steel. It can be possible by using Bimetallinc inserts. The file which I sent you for similar and dissimilar welding of aluminium and its different grades.



Thanks& Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282

E-mail : karthi...@yahoo.com

Reply all
Reply to author
Forward
0 new messages