can someone please tell me the tolerance between upper pressure gauge
reading and lower pressure gauge reading during hydraulic test witness
of pressure vessels as per ASME.
--
Thanks & Warm Regards,

Rahul Chaudhari
+918149199922


*P* *Think of the environment.*

*Please don't print this E- mail unless you really need to - this will help
preserve trees on the earth.*

José Juan Jiménez Alejandro

unread,
Apr 24, 2015, 1:06:20 PM4/24/15
to material...@googlegroups.com
Hydrostatic or pneumatic test pressure gauge needle must be in the middle third of the title page of this gauge, the details of the test you see them on UG-99 (VIII DIV 1) and PG-99 (I). Greetings!

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHjJ0V_A_UONNG_49nmDN%3D7TCy-7ui0Gz6QMtf9LEivGDVsjCw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--

Ing. Jose Juan Jimenez Alejandro

Cel. 8110834207; Next 16789654; ID 42*15*153815

Skype: jjjimeneza

Reply all
Reply to author
Forward
0 new messages