blind welded to pipe at test limit

53 views
Skip to first unread message

Jayasuryan Raveendran

unread,
Aug 6, 2015, 7:38:35 AM8/6/15
to material...@googlegroups.com

Dear frnds

For hydro test limit contractor does not have any blind flange or end caps so contractor requesting to diectly weld blind to the pipe. Is it acceptable. Any references for that. Constrtion code b31.3 test pressure 44 kgf per cm square

Regards
Jayasuryan

Don Under Survilliance

unread,
Aug 6, 2015, 8:04:06 AM8/6/15
to material...@googlegroups.com
yes offcourse he can weld it........



--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGt3MynrnPY%3D3LPhP2tw2s2c_s3tTGb410uvn7o1bbVyCqM75w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Bijay

unread,
Aug 6, 2015, 11:52:11 PM8/6/15
to materials-welding@googlegroups com
Yes blind can be welded directly to pipe but check the thickness of blind. 

Sent from Yahoo Mail on Android


From:"Don Under Survilliance" <dons...@gmail.com>
Date:Thu, 6 Aug, 2015 at 5:34 pm
Subject:Re: [MW:23279] blind welded to pipe at test limit

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM6T1-EQZUdNs%2B20EHz%2BUxN4n78qkHzHEoNx_CUHBmpuhkm00Q%40mail.gmail.com.

Asif Raza

unread,
Aug 6, 2015, 11:52:31 PM8/6/15
to material...@googlegroups.com

Dear it is not acceptable at all. Pl ask for the required standard and Specs which is valid as per the B31.1.

 

Peter

Welding Eng.

--

Jayasuryan Raveendran

unread,
Aug 7, 2015, 5:59:37 AM8/7/15
to material...@googlegroups.com

In b31.3 its mentioned only using blanks and spades  ,not welded blanks.

> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/55c35a77.691db50a.956bf.205aSMTPIN_ADDED_BROKEN%40gmr-mx.google.com.

Jayasuryan Raveendran

unread,
Aug 7, 2015, 5:59:44 AM8/7/15
to material...@googlegroups.com

Dear frnds

In design point of view is it acceptable. The weld joint will withstand the test pressure. ?