Dear experts,
I want to locate Fillet weld cracks below 6 mm for 22 mm plate with double V preparation.
Is there any special techniques from NDT I can use to identify cracks below 6 mm.
Please suggest me if any suitable NDT procedure for this. It is a bit urgent.
Appreciate your respond.
Regards,
Mohammed ghani.
Dear,
Thanks for the reply.
This is for RIG spudcan crack found after 3 years in service. .. I need to rectify if any more possible cracks available in fillet joints... usually with MPI we could locate cracks upto 5 to 6 mm...
Please prove me more suggestions.
Regards,
Mohammed ghani.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/h8u94emwh70urwdu19wnl0ig.1456666226993%40email.android.com.
From: Mohammed Ghani Sent: Δευτέρα, 29 Φεβρουαρίου 2016 - 05:19 Reply To: material...@googlegroups.com Subject: RE: [MW:24403] Fillet weld cracks below 6 mm with suitable NDT. |
After performing gauging, we found most of the cracks are below 6mm
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1346669f-f39d-4460-a282-dc42b4377911%40googlegroups.com.
Dear,
It is fillet weld for sure. ...
Regards,
Mohammed ghani.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANvSE6m_tZVX3%2B5-u-jbGYDg0D%2BHmeuTQpJUARQ3qzrMVf_cZg%40mail.gmail.com.
Dear experts,
I want to locate Fillet weld cracks below 6 mm for 22 mm plate with double V preparation.
Is there any special techniques from NDT I can use to identify cracks below 6 mm.
Please suggest me if any suitable NDT procedure for this. It is a bit urgent.
Appreciate your respond.
Regards,
Mohammed ghani.