Fillet weld cracks below 6 mm with suitable NDT.

44 views
Skip to first unread message

Mohammed Ghani

unread,
Feb 28, 2016, 5:47:39 AM2/28/16
to material...@googlegroups.com

Dear experts,

I want to locate Fillet weld cracks below 6 mm for 22 mm plate with double V  preparation.
Is there any special techniques from NDT I can use to identify cracks below 6 mm.

Please suggest me if any suitable NDT procedure for this. It is a bit urgent. 

Appreciate your respond.

Regards,
Mohammed ghani.

Agustin Jimenez

unread,
Feb 28, 2016, 9:18:29 AM2/28/16
to material...@googlegroups.com
Hello

I recomend Phased Array ultrasonic technic.

Agustín
Level 2 VT PT MT UT RT


Enviado desde mi smartphone Samsung Galaxy.


-------- Mensaje original --------
De: Mohammed Ghani <ghan...@gmail.com>
Fecha:28/02/2016 04:31 AM (GMT-04:30)
Para: material...@googlegroups.com
Cc:
Asunto: [MW:24396] Fillet weld cracks below 6 mm with suitable NDT.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVhBp4jWOun%3DrCPmJuh%2B1PLib%3D9%2BFM4KWDSsuRAUVRSVsg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Jayachandran

unread,
Feb 28, 2016, 10:18:56 PM2/28/16
to material...@googlegroups.com
Hello Sir,

I hope it is Butt weld T-Joint, so you can apply normal UT also.

Regards
Jayachandran V.

On Sun, Feb 28, 2016 at 1:01 PM, Mohammed Ghani <ghan...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (ghan...@gmail.com) Add cleanup rule | More info

Mohd Siraj

unread,
Feb 28, 2016, 10:19:00 PM2/28/16
to Materials & Welding
How u know crack is exactly 6mm below??

quite interesting.
Do RT.

Mohammed Ghani

unread,
Feb 28, 2016, 10:19:10 PM2/28/16
to material...@googlegroups.com

Dear,

Thanks for the reply.

This is for RIG spudcan crack found after 3 years in service. .. I need to rectify if any more possible cracks available in fillet joints... usually with MPI we could locate cracks upto 5 to 6 mm...

Please prove me more suggestions.

Regards,
Mohammed ghani.

dili...@gmail.com

unread,
Feb 29, 2016, 1:03:40 AM2/29/16
to Mohammed Ghani
I suppose you mean "verify" when you write "rectify". Unless you use huge magnets the max detection depth with MPI is no more than 2 mm

Sent from my BlackBerry 10 smartphone.
From: Mohammed Ghani
Sent: Δευτέρα, 29 Φεβρουαρίου 2016 - 05:19
Subject: RE: [MW:24403] Fillet weld cracks below 6 mm with suitable NDT.

Mohammed Ghani

unread,
Feb 29, 2016, 1:11:14 AM2/29/16
to material...@googlegroups.com

After performing gauging, we found most of the cracks are below 6mm

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.

Mohammed Ghani

unread,
Feb 29, 2016, 1:11:15 AM2/29/16
to material...@googlegroups.com

Dear,

It is fillet weld for sure. ...

Regards,
Mohammed ghani.

muthu barathi

unread,
Feb 29, 2016, 6:00:11 AM2/29/16
to material...@googlegroups.com


Dear Sir,

You may carryout with UT and sketch is attached



Thanking You.

With Warm Regards,

Muthu Barathi P.
Mobile : +919967300544 (Only message )
Mobile No. +965 50989210 (KUWAIT) after 8PM



From: Mohammed Ghani <ghan...@gmail.com>
Sent: Sun, 28 Feb 2016 16:17:38
To: material...@googlegroups.com
Subject: [MW:24396] Fillet weld cracks below 6 mm with suitable NDT.

Dear experts,

I want to locate Fillet weld cracks below 6 mm for 22 mm plate with double V  preparation.
Is there any special techniques from NDT I can use to identify cracks below 6 mm.

Please suggest me if any suitable NDT procedure for this. It is a bit urgent. 

Appreciate your respond.

Regards,
Mohammed ghani.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVhBp4jWOun%3DrCPmJuh%2B1PLib%3D9%2BFM4KWDSsuRAUVRSVsg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >
Untitled.png
Reply all
Reply to author
Forward
0 new messages