Dear All,
I need complete detail or reports for successful cladding welding ..
What are the quality controls usually applied for a cladding welding / pipe weld joint?
What are the possible problems that may occur during the welding of cladding?
The question raised based on avoiding even Single weld defects?
Thank you & Thank you very much.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_ncTF2Q%2Bt%2B6PKc1Pq6zpELvzNj%3DsMARhQpOvQSGjnxQUhQ%40mail.gmail.com.
Hello,
Please read this book. It covers various issues related welding of clad plates, pipes in great details. You may find answers to many of your questions here.
Regards.
Pradip Goswami.P.Eng, IWE.
Independent & Consulting Welding & Metallurgical Specialist
Saudi Aramco Approved Designated Welding Engineer(DPWR)
Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/
Email:pgos...@rogers.com,pradip....@gmail.com
Cell/Whasapp:1-905-9793232
From: PK M <pkm...@gmail.com>
Sent: April 23, 2021 10:55 PM
To: material...@googlegroups.com
Subject: Re: [MW:32321] I need complete detail or reports for successful cladding welding
Dear All,
I need complete detail or reports for successful cladding welding..
What are the quality controls usually applied for a cladding welding / pipe weld joint?
What are the possible problems that may occur during the welding of cladding?
The question raised based on avoiding even Single weld defects?
Special technique / Application
Sour Service & non Sour service.
Base material - A333 Gr 6 + UNS N06625, API 5L Gr B + UNS N06625, API 5L X52 PSL2 SMLS + UNS N08825
Pipe Size Range- 1. 0.5” to 8” Thickness -2.77 mm to 6.02 mm
2. 0.5” to 4” Thickness -3.73 mm to 8.56 mm
3. 6” & Above Thickness -10.97 mm to 30.18 mm
Application/ Process – GTAW + SMAW
Joint Type –Butt, Branch Conn, Fillet, Socket
Alloy Type -625 / 825
Clad/overlay – 3 to 5 mm
With PWHT / with PWHT
Applicable Code- ASME 31.3, Sec IX, SAES-0W-11
Thank you & thank you very much.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OjGAzTdpGELp5Axt%2BCXu-qhXV%2Bb75DQgMLq245nAKx-gA%40mail.gmail.com.
Dear All,
I need complete detail or reports for successful cladding welding..
What are the quality controls usually applied for a cladding welding / pipe weld joint?
What are the possible problems that may occur during the welding of cladding?
The question raised based on avoiding even Single weld defects?
Special technique / Application
Sour Service & non Sour service.
Base material - A333 Gr 6 + UNS N06625, API 5L Gr B + UNS N06625, API 5L X52 PSL2 SMLS + UNS N08825
Pipe Size Range- 1. 0.5” to 8” Thickness -2.77 mm to 6.02 mm
2. 0.5” to 4” Thickness -3.73 mm to 8.56 mm
3. 6” & Above Thickness -10.97 mm to 30.18 mm
Application/ Process – GTAW + SMAW
Joint Type –Butt, Branch Conn, Fillet, Socket
Alloy Type -625 / 825
Clad/overlay – 3 to 5 mm
With PWHT / with PWHT
Applicable Code- ASME 31.3, Sec IX, SAES-0W-11
Thank you & thank you very much.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OjGAzTdpGELp5Axt%2BCXu-qhXV%2Bb75DQgMLq245nAKx-gA%40mail.gmail.com.