RT Report clarification / advise required

121 views
Skip to first unread message

Mohammed Ismail

unread,
Apr 8, 2015, 10:30:50 PM4/8/15
to material...@googlegroups.com

Dear Experts,

 

I am pleased to draw your attention and please provide your valuable input / advice / comment / clarification regarding my interpretation as below.

 

The following is the requirement as referring to the attached 6600028289 (OOK) schedule Q_quality requirements attachment 1 clause 2.2.1.

 
Quote starts 


“ When performing, reviewing or ensuring Nondestructive Testing in VT, MT, PT, RT or UT, he shall be certified in the specific method(s). When performing, reviewing or ensuring Radiographic Testing Film Interpretation (), Inspector shall be certified in ASNT Level II."


Quote Ends

 

My interpretation is RT report shall be reviewed or ensured by the inspector with ASNT Level II certified in RTFI.

And after reviewing or ensuring the reports as per the requirements that report shall endorsed (singed) by that inspector who is qualified in RTFI .


But the vendor is dis agreeing with the my statement.

 

Please advise me. 


Thanks and best regards,

Mohammed Ismail,

Mechanical Inspector,

vendor inspection department,

Velosi.

6600028289 (OOK) schedule Q_quality requirements.pdf

Lakshman

unread,
Apr 8, 2015, 10:58:50 PM4/8/15
to material...@googlegroups.com
Hi friend, you are correct, but let us understand why client is not accepting and what is his views?
We should know theirs interpretation also prior to confirm...😊

Lakshman kumar.B
Project manager.
9440031459

From: Mohammed Ismail
Sent: ‎09-‎04-‎2015 08:00
To: material...@googlegroups.com
Subject: [MW:23061] RT Report clarification / advise required

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF2Z%3DtU1K6RTNjHkkjN1ibYNxK3VNSufzza5j4BgLah%2Bx%2BYAJg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

safad pp

unread,
Apr 12, 2015, 11:18:58 PM4/12/15
to material...@googlegroups.com
Dear Ismail,

please let us know whether you reviewed RT Report or RT film ? In
your quote RT report is mentioned only...

Shafad P.P
ASNT LEVEL 111 (RT,UT& MT)
India

Hareesh K V

unread,
Apr 12, 2015, 11:19:22 PM4/12/15
to materials-welding

Dear Sir,

You are correct and just for curiosity what is your vendors interpretation for that paragraph.

Regards,

Hareesh K V

Mohammed Ismail

unread,
Apr 13, 2015, 1:37:25 AM4/13/15
to material...@googlegroups.com
Dear Sir (s),

Thanks for involvement and providing valuable input/time in this regards.

This was highlighted to client in the inspection report, even though to ensure the finding i was seeking for advise.

In vendor point of view the RT report shall be reviewed and ensured by the inspector with ASNT level II certified in RT

Thanks and Best regards,
Mohammed Ismail,


On Fri, Apr 10, 2015 at 4:27 AM, Hareesh K V <haree...@gmail.com> wrote:

Dear Sir,

You are correct and just for curiosity what is your vendors interpretation for that paragraph.

Regards,

Hareesh K V

On Apr 9, 2015 8:28 AM, "Lakshman" <lakshma...@gmail.com> wrote:
Hi friend, you are correct, but let us understand why client is not accepting and what is his views?
We should know theirs interpretation also prior to confirm...😊
emoji_u1f60a.png

Mohammed Ismail

unread,
Apr 13, 2015, 1:37:25 AM4/13/15
to material...@googlegroups.com
Dear Sir,

This are RT report - final evaluation report / RT review form in which result of the RT were mentioned. Not the films.

For information these reports which is subjected for review were for the castings (eg; valve body /pump casing / cover).

with regards,
Mohammed Ismail

Thanks & Best Regards,

Mohammed Ismail

Inspection Engineer-Mechanical

Phone : +966 38394292 Ext - 243

Mobile + 966 565 063 994

Fax : + 966 3 8393671 

Velosi Saudi Arabia

Dammam-KSA.


Hareesh K V

unread,
Apr 13, 2015, 10:53:23 PM4/13/15
to materials-welding

Dear sir,

Please share with the vendor the guidelines of ASNT about level 2 in RT and RTFI.

RT qualification from ASNT Level 2 is an operator level qualification. In INDIA, an ASNT level 2 person cannot operate a radiography camera as we have to follow the regulations of AERB .Outside INDIA an ASNT level 2 person can operate a radiography camera.

In ASNT level 2 in RT there is nothing regarding the evaluation of radiography film.

An ASNT RTFI level 2 person is qualified to evaluate Radiography film, interpret it and is qualified to sign the report.

It is a general perception that an ASNT Level 2 in RT is qualified for film interpretation and that is wrong.

Best regards,

Hareesh K V

kingslygeo vargheese

unread,
Jun 11, 2015, 3:34:03 AM6/11/15
to material...@googlegroups.com
Dear Friends,
 
As per my understanding ASNT level - II have one qualification for  Radio Graphic Inspection which is ASNT LEVEL -II - RT.
which covers film review and reporting.
 
For Radio graphic film interpretation & Report authorization requires  ASNT LEVEL -II - RT.
 
The other qualification like MPI or LPE a level 1 operator can do that performing the MPI or LPE. Report evaluation and authorization by ASNT LEVEL -II MPI or LPE
 
But in RT film review Level-I cannot do.( Mostly in Middle east we are using Level- II for all including preforming MPI / LPE )
 
 
Kingsly Geo
Bureau Veritas
Abu Dhabi