Thickness reduction allowed in pressure vessel

58 views
Skip to first unread message

ABHISHEK SINGH

unread,
Feb 18, 2017, 9:45:01 PM2/18/17
to Materials & Welding
Dear Experts
How much thickness reduction Allowed in Shell of pressure vessel.

MOC-SA516GR65
Construction Code- ASME Sec.VIII

George Dilintas

unread,
Feb 19, 2017, 6:08:35 AM2/19/17
to Meghanadh K
mill underlolerance : Min(25 mm; 6% of ordered thickness)

In case of local thin areas see mandatory appendix 32


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9b33bcd1-ac72-4a70-a2e8-7cc8129d9cc7%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages