WPS QUERY

23 views
Skip to first unread message

prabhu

unread,
Aug 21, 2019, 4:06:42 AM8/21/19
to Materials & Welding
Hi experst,

I have qualified WPS of P1 G2 (grade LCC) can I use this WPS to weld P1 G1 (grade LCB) material.

I yes with which clause and if not why not?

George Dilintas

unread,
Aug 23, 2019, 11:35:25 PM8/23/19
to material...@googlegroups.com
If no impact test is required you can

Εστάλη από το Huawei κινητό μου


-------- Αρχικό μήνυμα --------
Θέμα: [MW:29976] WPS QUERY
Από: prabhu
Προς: Materials & Welding
Κοιν.:

Hi experst,

I have qualified WPS of P1 G2 (grade LCC) can I use this WPS to weld P1 G1 (grade LCB) material.

I yes with which clause and if not why not?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9209ad6e-56c5-407c-8f24-23d6568c4d53%40googlegroups.com.