Yes you can without a new PQR provided other parameters are within approval range
Sent from my BlackBerry 10 smartphone.
Original Message
From: JERRY TUAN
Sent: Κυριακή, 8 Νοεμβρίου 2015 - 06:13
To: Materials & Welding
Reply To: material...@googlegroups.com
Subject: [MW:23864] Revise was according to EN15614-1
If my pqr . I used butt joint double V, wire diameter 4.8 mm ,process SAW . Now I want to revise wps to used wire diameter 4.0 mm , is this ok
Thanks for help
Tuan.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/78a855f3-c4ca-4428-a39f-eaf687e97905%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
This message contains confidential information.
To know more, please click on the following link: http://disclaimer.bureauveritas.com