Thanks& Regards,
(Karthik)
Karthikeyan.S
E-mail : karthi...@yahoo.com
The only way to perform arc welding of such dissimilar combination is to use a transition piece of steel to Aluminum, produced by solid state welding process.
This article from ESAB , explains some of the problems of such welding.
Thanks.
P.Goswami.P.Eng, IWE.
Independent Welding & Metallurgical Specialist
Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/
Email:pgos...@quickclic.net,pradip....@gmail.com
Cell/Whasapp:1-905-9793232
From: 'Karthik' via Materials & Welding [mailto:material...@googlegroups.com]
Sent: May 23, 2019 10:07 PM
To: Materials & Welding <material...@googlegroups.com>
Subject: Re: [MW:29631] I need to do dissimilar weld joint (6xxx series Aluminium to Steel). What filler wire should I choose?
Hi,
The attached file might be useful to you.
Thanks& Regards,
(Karthik)
Karthikeyan.S
QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282
On Thursday, May 23, 2019, 6:44:48 PM GMT+7, Ram <rames...@gmail.com> wrote:
I need to do dissimilar weld joint (6xxx series Aluminium to Steel). What filler wire should I choose?
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7206cf51-d3f4-413a-838e-3036e9ad1a26%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1605684784.4306536.1558663626710%40mail.yahoo.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1605684784.4306536.1558663626710%40mail.yahoo.com.
Thanks& Regards,
(Karthik)
Karthikeyan.S
E-mail : karthi...@yahoo.com