1. Who will perform the classification test?
Flux & wire manufacturer
2. While reviewing the PQR, does the vendor need to submit Classification records?
The marking on the boxes / cans and the MTR is an evidence for classification
3. If a PQR is qualified with Flux Trade Name "X", can this PQR be used to support another WPS where Flux Trade Name "Y" is mentioned without classification? Please note, X & Y are from different manufacturer.
No
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE
Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Manas Ghosh ---11/05/2015 11:15:16---While qualifying a SAW Procedure as per ASME Sec IX, With respect to QW-404.9, the Flux Trade Name i
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6b0fedef-fe83-4f74-9e72-110cddda9bae%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
This message contains confidential information.
To know more, please click on the following link: http://disclaimer.bureauveritas.com