Generally why it is preferred to cut PQR piece transverse to the rolling direction of plate.What is the technical reason behind this??

dilintas

unread,
Jan 16, 2017, 10:45:00 AM1/16/17
to material...@googlegroups.com
Because rolled plates have anisotropic properties.
Thinkba little bit on grains orientation and you will find out why



Sent from my Samsung Galaxy smartphone.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/553dae23-e7b1-4100-874b-30038f99bf25%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages