Welder qualification

46 views
Skip to first unread message

Raghul

unread,
Aug 30, 2019, 2:53:08 PM8/30/19
to Materials & Welding
Welder made two coupon
1. Coupon with 6 mm thickness on the 1/2” pipe made by gtaw process
2.coupon with 15 mm thickness on 2-7/8” pipe made by gtaw+smaw process.

Is the welder qualify to weld on 1/2” pipe with gtaw+smaw process for qualified thickness?

Please explain

anand gupta

unread,
Sep 1, 2019, 12:44:55 AM9/1/19
to material...@googlegroups.com, Raghul
Dear 

We can use sa194 gr 7 nut in place of sa 194 gr 4 for low temperature carbon steel line. 

Regards 
--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.

Bien_ND / weldinginspections.net

unread,
Sep 8, 2019, 11:54:46 PM9/8/19
to Materials & Welding
which standard for qualification?

Mohit Aggarwal

unread,
Sep 8, 2019, 11:59:39 PM9/8/19
to materials-welding
If welder do welding on less than minimum 73 mm OD of pipe He able to qualify on minimum  1" pipe 25 mm OD pipe. Below 1" welder will have to do test on whatever doa required.


Kind Regards,
Mohit Aggarwal



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages