A106 GR B to A335 P11 Dissimilar welding

194 views
Skip to first unread message

Raja kumarasamy

unread,
Nov 1, 2020, 5:37:41 AM11/1/20
to Materials & Welding



Dear allr,




My project we have A106 GR B to A335 P11 Dissimilar welding ,Can any on suggest the PWHT and it's required?


t- 8.74mm
Dia: 2''












Regards

Raja kumarasamy
Multi Discipline Inspector (TPI)
ADNOC Waste Heat Recovery
ProjectRuwais, AbudhabiUAE

Kannayeram Gnanapandithan

unread,
Nov 1, 2020, 10:25:03 PM11/1/20
to materials-welding
As per ASME Section 1, it is not mandatory for thickness less than 16mm, provided preheat of 150℃ is to be done. Ref PW39

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1730221556.684444.1604222570928%40mail.yahoo.com.

SHOAIB ALAM

unread,
Nov 1, 2020, 10:25:05 PM11/1/20
to Materials & Welding
Dear sir
Please refer ASME B31.1 Table 132.2-1 Exemptions to Mandatory Post weld Heat Treatment

Manikandan J

unread,
Nov 1, 2020, 10:25:21 PM11/1/20
to material...@googlegroups.com
Code of construction?? 

George Dilintas

unread,
Nov 2, 2020, 4:00:23 AM11/2/20
to material...@googlegroups.com
If you Code of construction is either Asme viii-1, I, 31.1, 31.3 for this thickness the answer is NO