Orbital Tug welding in Cu Ni.

37 views
Skip to first unread message

Nazz A

unread,
Aug 31, 2015, 4:11:05 AM8/31/15
to Materials & Welding
Anybody did the Otbital tig welding by Polysoude machine. Now we are using an orbital machine for welding of Cu Ni pipes.

Please tell the good parameters of root welding.

prem_nautiyal26

unread,
Aug 31, 2015, 4:28:28 AM8/31/15
to materials-welding
Hi

You can get the parameters from the technical person of either your welding consumable supplier or machine supplier. 

Regards

Prem Nautiyal



Sent from Samsung Mobile
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a1a66a53-9722-449e-94e0-bbd494b8d2b7%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Nazz A

unread,
Sep 1, 2015, 3:08:24 AM9/1/15
to Materials & Welding
We have a brosure by Polysoude,the manufacturer. But the limitations are wide. Be cos the manufacturer parameters are commonly used for all material.

But everybody know about the parameters are related with position,size,thickness,metals, layers.

Anybody doing with the polysoude orbital machine, share the news about there.

george....@gr.bureauveritas.com

unread,
Sep 2, 2015, 2:59:23 AM9/2/15
to material...@googlegroups.com, mirto....@gr.bureauveritas.com

Dear all
in case you are interested for the following positions please submit detailed CVs and objective evidence for both experience and requested qualifications:

Lead Inspectors: 

Pipe mill inspector
 

    a. Proven experience with pipe manufacturing; 
    b. NDT (PT, MT UT and RT) Level II as per ASNT-SNT-TC-1A or equivalent; 
    c. Welding Inspector Level II as per CSWIP 3.1 or equivalent with experience in line welding process and spiral welding process.

Pipe mill coating inspector
 
    a. Proven experience with coating of pipes 
    b. NACE II or Frosio III or equivalent certification.

Pipe bends mill inspector
 
    a. Proven experience with pipe bends manufacturing; 
    b. NDT (PT, MT UT and RT) Level II as per ASNT-SNT-TC-1A or equivalent;

Pipe bends mill coating inspector
 
    a. Proven experience with coating for pipe bends 
    b. NACE II or Frosio III or equivalent certification.

In-line Inspectors
: 

Pipe mill in-line inspector
 
    a. Proven experience with pipe manufacturing; 
    b. Proven experience with in line welding proces and spiral welding process.

Pipe mill coating in-line inspector
 
    a. Proven experience with coating for pipes

Pipe bends mill in-line inspector
 
    a. Proven experience with pipe bends manufacturing;

Pipe bends mill in-line coating inspector
 
    a. Proven experience with coating for pipe bends

Handling supervisor
 
    a. Experience with pipe and pipe bends manufacturing/handling 
Clerck c/o Pipe Mill/Coating Mill 
    a. Experience with certificate traceability c/o Pipe Mill/Coating Mill 
best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

MW

unread,
Sep 2, 2015, 4:35:23 AM9/2/15
to Materials & Welding, mirto....@gr.bureauveritas.com
Request not to post any employment/job related posting here. there are many platforms to discuss these issues. for e.g you can post it  @ https://www.linkedin.com/groups?careerDiscussion=&gid=122787
it has wider reach there. 
Thanks 
Reply all
Reply to author
Forward
0 new messages