Dear Experts,
yes Mr. Muthu you are right and for CS the ppm is between 250 - 300 ppm.
Thanks,
Bala
On 10/25/16, muthu barathi <
muthu_...@rediffmail.com> wrote:
>
>
> Dear Sir,
>
> PH9 ok. But 25ppm is normally recommended for SS piping. For CS it could be
> in between 250 to 300 ppm and it could be found from your Project
> Specifications.
>
>
>
> Thanking you.
> With Regards,
> Muthu Barathi P. , Mobile number : 8469593553
> PH 9Clorines 25 ppm
>
>
> Sent from my Samsung Galaxy smartphone.
> -------- Original message --------From: Krisanu Bhunia
> &
lt;krisan...@gmail.com> Date: 23/10/2016 06:41 (GMT+02:00) To:
> Dear Expats,Please give information about hydro test water quality PH value
> and PPM limits for carbon steel and please give ref. code.regardskrisanu
>
> "Materials & Welding" group.