no problem, see aws d1.1 table 4.1 page 130. for more information see pre qualify wps .
Dear experts and seniors. If groove weld can cover for fillet weld, AWS D1.1 , can it cover for lap joint? Cause I read some where else in AWS D 1.1 that lap joint weld can be consider as fillet weld. Thanks all
--