No. Since its a non-pressure part.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
From: Shadab Ansari Sent: Δευτέρα, 31 Αυγούστου 2015 - 20:58 Reply To: material...@googlegroups.com Subject: Re: [MW:23374] PWHT requirement for vessel |
Is their any reference to code that says PWHT not required for non pressure parts. Or only pressure parts required PWHT.
Regards,
Prasad G.
vessel subject to pwht then weld prior n do pwht.
bcse any way skirt going to weld with pad which directly weld with vessels.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/38b09431-d6ff-43a2-ad04-3bbecd11b648%40googlegroups.com.
40 mm butt welds
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1441302561.90531.YahooMailBasic%40web142701.mail.bf1.yahoo.com.