MIG welding process-reg

68 views
Skip to first unread message

Karthikeyan Shanmugananthan

unread,
Apr 14, 2016, 6:57:05 AM4/14/16
to Materials & Welding
Dear Experts
Can we use MIG welding process for load carrying structural steel.... and also provide limitations of MIG welding process

Expecting your valuable suggestions

Regard
S.karthikeyan
Chennai

Alan Denney

unread,
Apr 17, 2016, 10:40:28 AM4/17/16
to material...@googlegroups.com
Yes you can, but not outside because the gas shield gets blown away. The big issue is lack of fusion defects. I hope that you have trained welders, qualified welding procedures and non-destructive testing, and that you are working to a recognised welding code of practice.

Alan Denney
AKD Materials Consulting Ltd
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d4a08674-c496-48d6-91df-9c49a35d8bd8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com


dili...@gmail.com

unread,
Apr 17, 2016, 10:40:38 AM4/17/16
to Karthikeyan Shanmugananthan
FCAW is better

Sent from my BlackBerry 10 smartphone.
  Original Message  
From: Karthikeyan Shanmugananthan
Sent: Πέμπτη, 14 Απριλίου 2016 - 13:57
To: Materials & Welding
Reply To: material...@googlegroups.com
Subject: [MW:24691] MIG welding process-reg

Jim Price

unread,
Apr 17, 2016, 10:41:46 AM4/17/16
to material...@googlegroups.com
The limitations of MIG welding has a lot of Depends:
1. Depends on Base Material.
2. Depends on Welding Wire
3. Depends on Shielding Gas
4. Depends on Welding Mode and Transfer
5. Depends on Heat Inputs
6. Depends on Joint Design

Jim Price | Welding Engineer, CWI
Direct:  320.7463439 | Fax: 417-862-5564
jimp...@polarcorp.com







-----Original Message-----
From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Karthikeyan Shanmugananthan
Sent: Thursday, April 14, 2016 5:40 AM
To: Materials & Welding
Subject: [MW:24691] MIG welding process-reg

Kannayeram Gnanapandithan

unread,
Apr 18, 2016, 1:25:00 AM4/18/16
to materials-welding

What is welding machine, if it is pulsed GMAW, u can use it for any thick, otherwise restrict to 13mm weld

Kannayeram Gnanapandithan

unread,
Apr 18, 2016, 1:25:12 AM4/18/16
to materials-welding

Mode of metal transfer plays a major role to choose this conventional GMAW process. If u have pulsed GMAW, in all current it will be in the pulsed spray mode only and u can use it for any thick, any position?

Vishwas Keskar Welding Manager Pune India

unread,
Apr 24, 2016, 11:50:42 PM4/24/16
to Materials & Welding
No issue .
Qualify PQR and use .
Use latest power source /wire feeder from reputed  welding equp manufactures

Kannayeram Gnanapandithan

unread,
Apr 25, 2016, 12:48:33 AM4/25/16
to materials-welding
if it is conventional power source, restrict to below 13mm or go for FCAW

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages