Hi Rajesh,
If it involves welding or Alloy 20 to same , them ER320LR is the matching & ideal consumable. ERNiCrMo-3 will be over matching as well as over priced. This filler could be used for dissimilar joints between alloy 20 and other alloys. Please seethe attachment for more details.
Pradip, what about 317 which has got more Mo than 320
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAAOLL9jWJnRlNiibrRouaze4BAAAAAA%3D%3D%40quickclic.net.
Dear sir,
Thank you very much for your reply.ER320 LR is not available in our area so can i use ERNiCr-3 for welding of alloy 20 ?
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d7b04f3b-f29e-4218-b302-3b1850f90e38%40googlegroups.com.