Hi all,

I'm doing some reasearch for a presentation and was wondering what
types of steel are best for specific jobs. For example a comersial
fisherman (folding or other wise), an outdoors man(fixed), kitchen use,
and general purpose/tachtical folding knife. Also I was hoping some one
could give me some help on the composition of various production knife
steels.

Thanks,
Jason


john

unread,
Jun 4, 1997, 3:00:00 AM6/4/97
to Matthew Donald Schallo

This is a multi-part message in MIME format.

--------------69D22767726E
Content-Type: text/plain; charset=us-ascii
Content-Transfer-Encoding: 7bit

Jason, I hope this helps.
John

--------------69D22767726E
Content-Type: text/plain; charset=us-ascii; name="steel chart.txt"
Content-Transfer-Encoding: 7bit
Content-Disposition: inline; filename="steel chart.txt"

The Knifemakers Steel Chart

by Carbon Manganese Chromium Nickel Vandium Molybdenum Tungsten
A.G.
Russell C Mn Cr Ni V Mo W

A-2 1.0 5.0

ATS34 1.05 0.4 14.5 4.0

AUS6A 0.65 1.0 14.0 0.5 0.1-0.2

AUS8A 0.85-1.0 1.0 14.0 0.5 0.1-0.2 0.1-0.3 0.4

CPM440V 2.15 0.4 17.0 5.5 0.4

154CM 1.05 0.5 14.0 4.0

1095 0.95 .25-.55

D-2 1.05 0.06 12.5 0.3 1.10 0.7-1.3 0.4-0.6

52100 1.10 0.4 1.5

O-1 0.85-1.0 1.0-1.5 0.4-0.6 0.3 0.3

Sandvic
12C27 0.6-0.7 0.37 14.0

440A 0.6-0.8 1.0 14.5 0.75

440C 0.95-1.2 1.0 14.5 0.75

420
Modified 0.3-0.5 1.0 12.0-14.0 0.5

T425
Modified 0.65 0.35 13.5 1.0

420 0.15-0.35 1.0 12.0-14.0

by C Mn Cr Ni V Mo W
A.G.
Russell Carbon Manganese Chromium Nickel Vandium Molybdenum Tungsten

We do not list Phosphorus, Sulfer or Silicon as these are undesirable
elements in fine tool steels used for knives. Makers should buy their steel
from the supplier who includes the least amount of them.

---------------------------------------------------------------------------
---------------------------------------------------------------------------
---------------------------------------------------------------------------
[Image]
[Image]
Toll Free 800-255-9034
Fax 501-751-4520
MasterCard - Visa - Discover

---------------------------------------------------------------------------

[Home] [Guarantee] [FAQ] [Knife Care] [Catalog]

This page, and all contents, are Copyright © 1996 by A.G. Russell -
Springdale, Arkansas.

--------------69D22767726E--


0 new messages