WPS, Welder and NDT Qualification for High Pressure Piping (ASME B31.3, Chapter IX)
Design Code: ASME B31.3, Chapter IX (2010)
Scope of work: 1. Procuring the material as per the attached material datasheet.
2. Carryout Chemical and HIC tests (as per SP 2041 acceptance criteria: Region 3 service) on the procured material
3. Submit proposed WPS (PWPS) for project team approval
4. Cutting and welding the test coupon as per approved PWPS.
5. Carrying out PWHT, NDT, Mechanical tests as per approved PWPS and ASME B31.3, Chapter IX.
6. Submit NDT procedure, technique sheets for PDO approval.
7. NDT technicians shall be approved by PDO
Data Sheet
Description |
|
Specified | |
Design Code |
ASME B 31.3, Chapter IX (2010) | ||
Dimensional spec |
ASME B36.10 | ||
Service |
GAS - HIGH SOUR, ONSHORE | ||
Design Pressure |
495 bar g | ||
Min. Design Temperature |
MINUS 50°C | ||
Max. Design Temperature |
PLUS 180°C | ||
Mat |
CARBON STEEL FINE GRAINED | ||
Mat, spec |
ASTM A333 GR 6 | ||
Material Technical Spec. |
NACE MR 01-75/ISO 15156 | ||
Manufacturing process |
SEAMLESS | ||
|
| ||
End Preparation |
Beveled, ASME B16.25 | ||
Inspection, certificate |
ISO 10474 -3.1C | ||
Notes:
1. Pipe wall thickness is calculated based on ASME B 31.3, Chapter IX, clause K 304.1.2.
2. Manufacture and supply of pipe shall be in accordance with ASTM A333 GR.6 and this specification.
3. Impact testing shall meet the requirement of ASME B31.3, Chapter IX, clause K 323.3.1
4. 100% ultrasonic examination as per ASME B 31.3, Chapter IX, clause K 305.1.2
5. All pipes shall be procured from PDO approved vendor.
MESC No. |
Piping Class |
Size DN |
Wall Thickness |
743016711X |
1001503P1 |
600 |
108mm |
|
|
|
|
|
|
|
|
Regards
VENKAT