IS2062 has been included in ASME BPV Sec IX 2011 addenda under P number 1 Group number 1 for all the three grades (i.e. A,B,C) [cid:image002.png@01CC7A0B.4059AEF0] From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING) Sent: Monday, January 31, 2011 9:12 AM To: 'materials-welding@googlegroups.com' Subject: RE: [MW:9569] P1 no Range IS 2062 is an unlisted material SS 410 will under P number 6 ( refer table QW/QB 422) From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of puneet takiar Sent: Sunday, January 30, 2011 8:04 PM To: materials-welding@googlegroups.com Subject: Re: [MW:9565] P1 no Range Hello! Can anybody tell me in which P. no IS 2062 grade A and SS 410 will fall and how to search in ASME sex IX table. Regards, Filtered by Hosted Filtering