Contamination of silver by chlorine?

40 views
Skip to first unread message

Al Slavin

unread,
Jan 24, 2012, 2:40:04 PM1/24/12
to surface...@googlegroups.com, Al Slavin
I have found that the silver electrodes on commercial QCM crystals develop a strong 181-eV Auger peak after they have been cleaned by ion bombardment and then allowed to sit in vacuum for several hours at 35 C or above. I SUSPECT that this peak is from chlorine which is a contaminant in the silver and segregates to the surface on heating.

Can the chlorine be removed by extended annealing in a reactive gas? What gas would be best?

Any other suggestions?

Alan Slavin

nadir

unread,
Feb 7, 2012, 9:31:11 AM2/7/12
to Surface Science
Hi Alan,

I am not sure but atomic hydrogen might be able to remove Cl
contamination on silver surface even without annealing.

Nadir Faradzhev

nadir

unread,
Feb 7, 2012, 10:09:12 AM2/7/12
to Surface Science
Al, please note that I suggested to use atomic hydrogen. To split
molecular hydrogen into two atoms you need some energy (e.g. ~ 1800
degrees on tungsten filament). Unless a heated silver will do it for
you, the reaction yield is expected very low. Nadir


On Jan 24, 2:40 pm, "Al Slavin" <asla...@trentu.ca> wrote: