Google Groups no longer supports new Usenet posts or subscriptions. Historical content remains viewable.
Dismiss

EVA

0 views
Skip to first unread message

annamaria romeo

unread,
Oct 1, 1997, 3:00:00 AM10/1/97
to

I'm looking for physical and chemical properties of EVA
(ethylen-vinylacetate, 37% VA). More specifically, I'm interested in :
1) flammable point
2) ignition point
3) thermal conductivity
4) heat capacity.
Do you know where I can get safety data sheets of polymers?
Thanks a lot
AR

Ken C Wurtzel

unread,
Oct 13, 1997, 3:00:00 AM10/13/97
to

Try Dupont: 302-774-0821

annamaria romeo <Annamar...@cselt.it> wrote in article
<343249...@cselt.it>...


> I'm looking for physical and chemical properties of EVA
> (ethylen-vinylacetate, 37% VA).

William R. Behymer

unread,
Oct 14, 1997, 3:00:00 AM10/14/97
to

You might also try Millennium Petrochemicals. Their web site is at
http://www.millenniumpetro.com/

Dennis Falkenstrøm

unread,
Oct 15, 1997, 3:00:00 AM10/15/97
to

Hello All

I want to use a FT-IR spectrofotometer to determin the EVA % in PE.
But first of all I need at method to determin the EVA by titration.
Does anybody know such method ?
--
Dennis Falkenstrøm
Chemistry, Laboratory, Alife, C64, Music.
http://home5.inet.tele.dk/dennis-f/index.html