You might also look at the current edition of _Metallurgical
Thermochemistry_, by Kubaschewski and various co-authors (Evans and
Alcock for the 4th, I think just Alcock for the 5th, which is the last
I've seen). It has extensive tables of numerous thermodynamic
quantities, including vapor pressures and Gibbs energies of formation.
Joe Long