Does anyone have information about a possible alloy that might form
when using the electroless nickel, electroless palladium, immersion
gold surface finish and a solder alloy that might form with tin based
solders. Specifically, does anyone have information or phase diagrams
on the potential gold-palladium-tin alloy that might form? Any
assistance or data would be appreciated.