Does anybody know of a source for Invar 36 in thin sheet form? Any
help would be appreciated.
Ron
Does anybody know of a source for Invar 36 in thin sheet form (about
0.030" thick) and in small quantities ? Any help would be
appreciated.
Ron
Tried Special Metals - Wiggin ?
Steve
Thanks Steve, but no joy there.
try
Contact Us:
High Temp Metals, Inc.
12910 San Fernando Rd.
Sylmar, CA 91342-3601
Phone: 800-500-2141
818-362-5357
Fax: 818-362-9884
sa...@hightempmetals.com
Hi Bob,
Any NiSpan-C in the same sort of thickness, per chance ?
I have a little project that has stalled for years for the lack of it !
Steve
steve-
I don't know what Ni-SpanC is.......
give these folks a call or drop them an email
www.matls.com is a good site for finding suppliers
cheers
Bob
> steve-
>
> I don't know what Ni-SpanC is.......
>
Its another exotic nickel alloy with a virtually zero coefficient of
elasticity with temperature.
Steve
Sorry I didn't read the header in your post. My US sources won't be much help
in the UK.
Cheers
Bob
Please check :
http://www.thyssenkruppvdm.com/Info_Dienst_pdf_01_eng.html#Ausdehnung
Look at Pernifer 36.