http://igor.chudov.com/projects/Diamond-Wheel-Grinder/

My main intention is to save my drill doctor for drills, and to grind
tungsten electrodes with this grinder. Some details are on that page.

The diamond wheel was acquired on eBay.

Would be interesting to know how old this peerless motor is. It says
frame CE12C.

i

Potblak

unread,
Aug 18, 2006, 7:16:43 AM8/18/06
to
So where do you collect the carcinogenic Thoria dust?

"Ignoramus23953" <ignoram...@NOSPAM.23953.invalid> wrote in message
news:oQbFg.24847$6C....@fe60.usenetserver.com...

Nick Müller

unread,
Aug 18, 2006, 9:33:15 AM8/18/06
to
Potblak <Inv...@Invalid.net> wrote:

> So where do you collect the carcinogenic Thoria dust?

Didn't you see the transparent disk guard with the connector to the
vacuum cleaner? ;-))


Nick
--
The modular DRO
Available now in USA / Canada
<http://www.yadro.de>
..|....|....|....|....|....|....|..

Ignoramus23732

unread,
Aug 18, 2006, 9:48:34 AM8/18/06
to
On Fri, 18 Aug 2006 21:16:43 +1000, Potblak <Inv...@Invalid.net> wrote:
> So where do you collect the carcinogenic Thoria dust?

I figure that if I use it once or twice a week, there is not that much
danger to me. Still, I will try to fashion some sort of a vacuum
cleaner hose holder of some sort, as well as electrode support.

i

dca...@krl.org

unread,
Aug 18, 2006, 10:55:24 AM8/18/06
to

Potblak wrote:
> So where do you collect the carcinogenic Thoria dust?
>
> > i
> >

You don't have to use tungstens with thoria. In fact they are not the
best ones to use.


Dan

Ignoramus23732

unread,
Aug 18, 2006, 11:16:57 AM8/18/06
to
On 18 Aug 2006 07:55:24 -0700, dca...@krl.org <dca...@krl.org> wrote:
>
> Potblak wrote:
>> So where do you collect the carcinogenic Thoria dust?
>>
>
> You don't have to use tungstens with thoria. In fact they are not the
> best ones to use.

I have some lanthanated ones. Dangers of thoria, though, should not be
overstated for a weekend warrior like me. I am not production welding
and I am not sharpening tnugstens every 5 minutes. I do it once a
week or so.

Still, I think, I will make some changes to this and will add a shop
vac hose holder of some sort and an adjustable holder.

i

JR North

unread,
Aug 18, 2006, 6:50:59 PM8/18/06
to
I collect mine in my lungs...
JR
Dweller in the cellar
glowing happily

Potblak wrote:


--
--------------------------------------------------------------
Home Page: http://www.seanet.com/~jasonrnorth
If you're not the lead dog, the view never changes
Doubt yourself, and the real world will eat you alive
The world doesn't revolve around you, it revolves around me
No skeletons in the closet; just decomposing corpses
--------------------------------------------------------------
Dependence is Vulnerability:
--------------------------------------------------------------
"Open the Pod Bay Doors please, Hal"
"I'm sorry, Dave, I'm afraid I can't do that.."

JR North

unread,
Aug 18, 2006, 6:55:20 PM8/18/06
to
Here's mine:
http://www.harborfreight.com/cpi/ctaf/displayitem.taf?Itemnumber=94071

JR
Dweller in the cellar

Ignoramus23953 wrote:

Ignoramus23732

unread,
Aug 18, 2006, 8:25:56 PM8/18/06
to
On Fri, 18 Aug 2006 15:55:20 -0700, JR North <jason...@bigfoot.com> wrote:
> Here's mine:
> http://www.harborfreight.com/cpi/ctaf/displayitem.taf?Itemnumber=94071

Do you grind tungstens with that thing? What are the wheels made of ??

i