I think it was not working because they didnt know how to start the
arc.. pilot arc system, no HF
They managed to burn up the electrode, diffuser and nozzle..and maybe
the torch head itself.
Daytona Mig wants $125 for the head, and about another $25 for
consumables
Anyone point me to a cheaper source, or someone have leftover
consumables after they upgraded to a more powerful machine?
This does have power...forms the plasma in the head because of the
burned consumables and diffuser.
Thanks in advance
Gunner
Political Correctness
A doctrine fostered by a delusional, illogical liberal minority and
rabidly promoted by an unscrupulous mainstream media,
which holds forth the proposition that it is entirely possible
to pick up a turd by the clean end.
"Gunner" <gun...@lightspeed.net> wrote in message
news:sk03u2pe5s93ubtuh...@4ax.com...
Gunner is so good at scrounging, he can probably even get paid for
taking great stuff. Heis the God Almighty of scrounging. I wish I was
that good!!!
i
who just bought two large crates full of new motors for 50 cents apiece
>You get a FREE plasma cutter.
>It only costs $150 to fix it up, and you want CHEAPER??????
>
Of course! Im a scrounger, not a retail shopper!!!
<G>
Gunner
"Liberalism is a philosophy of consolation for Western civilization as it commits suicide"
- James Burnham
>On Tue, 27 Feb 2007 10:13:33 +1100, Potblak <Inv...@Invalid.net> wrote:
>> You get a FREE plasma cutter.
>> It only costs $150 to fix it up, and you want CHEAPER??????
>
>Gunner is so good at scrounging, he can probably even get paid for
>taking great stuff. Heis the God Almighty of scrounging. I wish I was
>that good!!!
Actually..I was paid to take 30 gallons of high sulpur cutting oil. And
they put it in nice new 5 gallon gas cans too.
Works great in the lathes. Little smokey though....<G>
The oil was from a demo at Westec a few years ago...<G>
>
>i
>who just bought two large crates full of new motors for 50 cents apiece
What kind?
Gunner
>
>> "Gunner" <gun...@lightspeed.net> wrote in message
>> news:sk03u2pe5s93ubtuh...@4ax.com...
>>> Guy gave me a non working plasma cutter. Daytona Mig Pocket 25 made by
>>> Cebora.
>>>
>>> I think it was not working because they didnt know how to start the
>>> arc.. pilot arc system, no HF
>>>
>>> They managed to burn up the electrode, diffuser and nozzle..and maybe
>>> the torch head itself.
>>>
>>> Daytona Mig wants $125 for the head, and about another $25 for
>>> consumables
>>>
>>> Anyone point me to a cheaper source, or someone have leftover
>>> consumables after they upgraded to a more powerful machine?
>>>
>>> This does have power...forms the plasma in the head because of the
>>> burned consumables and diffuser.
>>>
>>> Thanks in advance
>>>
>>> Gunner
>>>
>>> Political Correctness
>>>
>>> A doctrine fostered by a delusional, illogical liberal minority and
>>> rabidly promoted by an unscrupulous mainstream media,
>>> which holds forth the proposition that it is entirely possible
>>> to pick up a turd by the clean end.
>>
>>
"Liberalism is a philosophy of consolation for Western civilization as it commits suicide"
- James Burnham
I am impressed. Probably stinks a lot though.
>>i
>>who just bought two large crates full of new motors for 50 cents apiece
>
> What kind?
Fractional and full horsepower, short and long shafts, some with gear
reducers, most not, most single phase.
i