A number of individuals are in progress of comparing a P/M D2 blade
(Spyderco Military) against a wrought D2 blade (Mel Sorg). The first
evaluation has been completed by Michael Cheshareck and can be seen
here :

http://www.cutleryscience.com/forum/read.php?7,23,23#msg-23

I have also finally put up the home page :

http://www.cutleryscience.com/home.html

and am finally getting the website together. Anyone who wants to
contribute would be appreciated as always.

-Cliff

bruce...@gmail.com

unread,
Aug 16, 2007, 8:50:26 AM8/16/07
to

There is a dissertation entitled:

Experiments on Knife Sharpening
John D. Verhoeven
Emeritus Professor
Department of Materials Science and Engineering
Iowa University
Ames, IA

available on the web that might be of interest to your readers.


Bruce in Bangkok
(brucepaigeATgmailDOTcom)

Cliff

unread,
Aug 16, 2007, 10:38:09 AM8/16/07
to
On Aug 16, 10:50 am, brucedpa...@gmail.com wrote:
> There is a dissertation entitled:
>
> Experiments on Knife Sharpening
> John D. Verhoeven
> Emeritus Professor
> Department of Materials Science and Engineering
> Iowa University
> Ames, IA

Thanks, I have added that and some other articles to the appropiate
page now. I will be expanding them shortly with links into the
discussion forum to allow critical feedback on that work. Ref :

http://www.cutleryscience.com/articles/index.html