Thanks in advance...
SC
> Does anyone know whether lapis lazuli is heat sensitive? What I really need
> to know is whether it's ok to heat it to the temp necessary to get dop wax to
> stick, or whether I should use cold dopping instead.
>
It is okay to heat it. A good general rule for any stone is to get the
stone no hotter than you can hold with your fingers.