Chuck the old one (after testing the new one) and get back to work.
An odd symptom. You don't say whether your flame is now withough air, giving a
soft yellow and sooty flame, or if it's simply a normal flame which has just
changed color. The two symptoms are different. Plus, is the flame color
orange, or a that shade of yellow you get when the flame flows over a fluxed
surface at soldering temps?
But anyway...
The Smith "Handi-heat" air/acetylene torches mix air with the fuel gas through
orifices/vents in torch, with each tip having it's own such vents. That means
that the proper mix of air and acetylene is performed by each tip. If two
seperate tips both produce the problem, then it's unlikely that the air/fuel
mixing arrangement is the problem, with one exception. In order for these tips
to work, there does need to be sufficient fuel gas pressure to get enough fuel
to the tip in the first place. But you'd know easily if this was the problem,
since then you'd have little or no flame at all. That your problem is just that
the flame has changed suggests to me that the tip is getting the needed gas, and
an appropriate pressure. So the torch tip, and probably the torch, which is
just a valve feeding gas to the venturi and orifice on the tip section, is
probably working right.
Now, the regulator handles only the gas pressure. If it were not working, your
pressure would vary, motorboat, not work, leak, or something like that. In
order to get a yellow flame rather than the normal blue one, you need to either
have not enough air, or some foreign chemical added to the fuel gas which would
color the flame, regardless of the fuel/air mix. As the regulator has no way of
reducing the air in the fuel mix, since there isn't yet any air in the mix until
the tip itself introduces it (any regulator error here would be to increase the
air in the mix, giving too hot a flame, not a yellow/orange one. And I'm not
even sure if it's possible to mess up a regulator enough to get air into the mix
at all. All I've ever seen were regulators that leaked gas, didn't let gas
flow, or didn't let it flow evenly, or the like.) So to me, that means
something foreign is getting into the gas flow by the time it's being burned, or
something in the gas is interfering with the normal operation of the tip.
One obvious possibility that occurs to me is that anything containing sodium,
like salt, or more likely, most of the fluxes we use which include borax, will
give a bright yellow/orange color to a normal flame if it is introduced into the
flame. A torch tip with a bunch of flux spilled and dried onto the end of the
tip would do this, for example. Normally, such chemicals are not vapors without
heating or some sort of solvent, so simply spilling some flux on a regulator,
even if it somehow got inside, might not color the flame. The chemical needs to
be in vapor form or otherwise able to be carried along with the gas flow. And
THAT leads me to wonder if something is contaminating the gas itself in your
tank. Acetylene is dissolved in acetone in the tank. I'm wondering if you've
somehow got a tank where, for example, something else is also in there as a
trace contaminant. That might then give an effect similar to a vapor fluxing
unit, where simply bubbling the gas through a solvent containing flux introduces
a little flux to the flame, along with a color from it. The so-called "water"
torches, for example, produce an oxy/hydrogen flame that, were it purely oxygen
and hydrogen, would be almost colorless and rather hard to see. But they are
not so, due to the use of solvent fluxes, which can, in some cases, give a quite
green or yellow tinged flame if a boric acid or borax containing flux is used...
Even more, if some such agent were contaminating your acetylene tank, then that
agent might also make the venturi/air vent structure of the tips operate
incorectly, so installing a different tip might still produce the colored/odd
effect...
My vote goes not for a faulty regulator, but for a faulty acetylene tank...
Hope this helps.
Peter Rowe
Well, now you've stumped me too. You state that there is a small blue cone,
which sounds like a normal proper flame. but such a flame would not be too cool
to solder, nor would it be brushy and orange. I'd normally expect an oxygen or
air starved flame, which would indeed be orange/yellow and brushy, to NOT have
that small blue cone. So this just sounds weird. I think at this point the
only suggestion I've got is to start substituting various other parts from
another torch to see which replacement part fixes the problem. To do that, of
course, it will be helpful to borrow another torch from another jeweler who uses
one, if you can find such a person locally. If you're anywhere near Seattle,
you can borrow mine...
Peter Rowe
If they can't answer your question, then you've got real problems.
If you're in NYC, bring it by Metalliferous (34 West 46th Street). I'll
take a look.
David
The only other thing I can think of is that you accidentially bumped the
valve on one of your regulators and are getting the gas at a lower pressure.
This really doesn't explain alot of your symptoms but is worth a look before
buying a new one. Are the tips clean and clear of debris?