> We have just completed our first production run on a visor type with
> AUR-92 flat plate and ratchet headgear to take the weight off of you
> nose. Initial feedback from the first customers is that it is great!!!
> Bob Aurelius CEO AURA LENS PRODUCTS
I recently purchased this visor and I love it! Previously, I had used
didymium clip-ons because I wear glasses. The clip-ons were heavy and I
did not want to possibly ruin my regular glasses with the clips, plus
they were very heavy. The visor not only has the AUR-92 lense, which is
superior to didymium, but moves the lense away from my glasses. I can
now use my regular everyday glasses, instead of an old pair (& old
prescription) and also if I need to, I can use my magnifiers on my
glasses as well.
Jean
Don McKinney
Ingrid
Hi Ingrid,
First and foremost we do not use the rose dd glass in our new visor, the
material is the AUR-92 glass tempered for additional protection. The
price is $160.00
Thanks for your interest. We have stock on hand and can ship in one day.
You can see our first model in our site at www.auralens.com. under
simple magnification.
Bob Aurelius