Many a times I face a problem of Selecting Bolting Material Impact
tested as per PED ( i.e. with 54J Energy at Lowest Schedule operating
temperature).
Let me know which material is best when I shall be using it for (-) 25
Deg C
As I understand SA193 Gr B7 which is readilly available cannot give
52J below 10 Deg C. EN19 is preferred material for this before Heat
treatment.
If I am correct,SA320 Gr L7 which is gives 52J below -25 Deg C. But
what shall be raw material for this grade before heat treatment.
Regards
Rajesh Bhavsar
Bathula Raghuram (Mumbai - PIPING)
unread,
Jul 10, 2008, 12:24:38 AM7/10/08
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to PED...@googlegroups.com, material...@googlegroups.com
SA320L7/SA194 Gr4 combination also can be used (no matter what raw material they use, generally it is from SA29, AISI 4140..._), one need to specify and MDMT and energy requirements while ordering.
Haldor Topsoe spec recommends DIN17290/26CrMo4/1.7219 for -11 to -60 deg.C, may check the equivalents as it is a very old one and the std might be obsolete now.
Please share other alternate/equivalent standards for LT application