Excess weaving in FCAW welding process

109 views
Skip to first unread message

RAJESH KUMAR

unread,
Oct 2, 2023, 8:59:39 AM10/2/23
to materials-welding, Rajesh Kumar
Dear Experts,

Code:BSEN 15614-1:2017 ,BSEN 15609:2019 and DNV-OS-C401

I have noticed that WPS says the weaving is allowed/permitted 18 mm maximum for FCAW welding process.Please tell me whether we can allow if the weaving is more than the allowable limit.If it can be allowed.What is the reasons and on what basis it is allowed?If it can not/should not be allowed.Why and what is the reasons?


Thanks & Regards

Rajesh kumar
Dubai.

RAJESH KUMAR

unread,
Oct 5, 2023, 10:00:39 AM10/5/23
to materials-welding, Rajesh Kumar
Dear Experts, 

The contractor is of the opinion that It is not an essential variable, hence it can be allowed. To substantiate their claim they say they will change the WPS and they will perform a hardness Test to prove that the properties were not changed. Please advise.

Best regards
Rajesh
--



Thanks & Regards

Rajesh kumar
055-5251449
Sharjah

madheswaran s

unread,
Oct 5, 2023, 10:00:39 AM10/5/23
to material...@googlegroups.com, Rajesh Kumar
Excess weaving will tend to rise Heat input more so, Toughness will be reduced. Mechanical property will change as said above. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMtcSfPVaUrZpa-zbt1cQ0%3DcLD5g6OuEVPkDv36KTkbeZUsghg%40mail.gmail.com.

Kannayeram Gnanapandithan

unread,
Oct 5, 2023, 10:00:44 AM10/5/23
to materials-welding, Rajesh Kumar
welder became in fatigue stress in handling the torch. 18mm is the dia of nozzle approximately 

Vishwas Keskar

unread,
Oct 6, 2023, 4:52:32 AM10/6/23
to material...@googlegroups.com, Rajesh Kumar
Is impact testing is required as per drawing ??

Sent from my iPhone

On 05-Oct-2023, at 7:30 PM, Kannayeram Gnanapandithan <kgpan...@gmail.com> wrote:



RAJESH KUMAR

unread,
Oct 10, 2023, 3:42:56 AM10/10/23
to material...@googlegroups.com, Rajesh Kumar
Yes, as per drawing design temperature is 0 degree celsius.  

Best Regards,
Rajesh



--




Best Regards,
Rajesh Kumar
Dubai.