Can we use SS spiral wound gasket(316L-inner Ring) for the both CS connecting flanges, I am working in a petrochemical where all the spiral wound gaskets used were SS.Do any code specifies the use spiral wound gasket to particular materials or is it a choice of owner/user.

Kristian Lund Jepsen

unread,
Feb 6, 2016, 4:22:02 AM2/6/16
to material...@googlegroups.com

You can use the SS spriral wound gasket with 316L inner ring for CS connecting flanges.

Many oil companies have that as part of their piping specifications, and it does not compromise any codes or standards.

 

Because you have small amounts of stainless steel in large carbon steel piping systems, you will basically not have a galvanic corrosion problem.

 

Regards

Kristian

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/def915ef-a7fe-4dfc-a1d6-c4b1d29dd395%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

dili...@gmail.com

unread,
Feb 6, 2016, 4:22:04 AM2/6/16
to Meghanadh K
You have to check the eventuality of galvanic corrosion due to difference of potential.
Dr. G. Dilintas
AIS, AIN

Sent from my BlackBerry 10 smartphone.
From: Meghanadh K
Sent: Σάββατο, 6 Φεβρουαρίου 2016 - 06:23
To: Materials & Welding
Subject: [MW:24234] ss spiral wound gasket to cs flanges
Can we use SS spiral wound gasket(316L-inner Ring) for the both CS connecting flanges, I am working in a petrochemical where all the spiral wound gaskets used were SS.Do any code specifies the use spiral wound gasket to particular materials or is it a choice of owner/user.

--

Mohd Siraj

unread,
Feb 7, 2016, 3:57:17 AM2/7/16
to Materials & Welding
reason for do so is graphite lining on spiral lining gasket has perfect contact with CS raised face.