Good morning every body,

Following your knowledge and your experience, please advise me how to determine the nitrogen evaluation rate (NER) for the cryogenic tank.

My question:

-          Is there any code to control the NER?

If no code any procedure or specification on the subject would be appreciated.

Also, following the Manufacture’s Data Report for the tank, the acceptance standard maximum is 150 mtorr for 72 hours. Is this value (150 mtorr) mentioned in the codes and standard or just manufacturer’s standard?

Thanks in advance.

 

George Dilintas

unread,
Feb 22, 2017, 10:39:25 PM2/22/17
to Meghanadh K
Evaluation or Evaporation?

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/63f9a5df-b0fe-4748-a549-4f33e14cab74%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Brl Pp

unread,
Feb 27, 2017, 10:14:54 PM2/27/17
to Materials & Welding
Hi M. Georgios Dilintas,

Thanks for your replay.

I correct, Evaporation not Evaluation

For help, I need your experience about the Evaluation of NER by pressure rise methode.

Your response for my preocupation is helpful.

Thanks in advance.

Benadjal Redouane
Mechanical engineer Sonatrach algeria