Dear All,
Does butt weld WPS is applicable for socket weld? Can anyone provide ASME IX code reference for this ?
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0490206d-a0a5-4fdd-a513-645d5fc1eaad%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Sorry to disagree –a socket weld is simply a fillet weld and a WPS can be written from a groove weld PQR to cover all fillet welds in addition to groove welds. See Table QW-452.6. Fillet welds must be referenced on the WPS and additional information for setting up the socket weld will have to appear on fabrication drawings or be included on the WPS (i.e. the 1/16 inch gap prior to performing the weld). A separate WPS for each weld configuration is not required by ASME – typically referenced to fabrication drawings.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/0490206d-a0a5-4fdd-a513-645d5fc1eaad%40googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAK-7o_Mz8-%2B%3DuRQm9O_%2B%3DNLDZbZZ1Zgr_T%2BZg%3Dhf1iQOr2Cbnw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/tvyiixqpkstxrtm3rh44eqym.1484664204175%40email.android.com.
Dear All,
Does butt weld WPS is applicable for socket weld? Can anyone provide ASME IX code reference for this ?
If they are an experienced fabricator, the 2mm gap is understood, of course that is assuming proper pipe fitting/fabricating training. Many shop detailers of isometrics may not even know about the gap, so it doesn’t get put in the isometric drawing notes.
L.G. Murrell, Jr-“Butch”
Coastal Machine & Mechanical, LLC
Email: bmur...@coastalmandm.com
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9b1vldnqswaaeqx5rd35iebh.1484805745544%40email.android.com.
If they are an experienced fabricator, the 2mm gap is understood, of course that is assuming proper pipe fitting/fabricating training. Many shop detailers of isometrics may not even know about the gap, so it doesn’t get put in the isometric drawing notes.
L.G. Murrell, Jr-“Butch”
Coastal Machine & Mechanical, LLC
Email: bmur...@coastalmandm.com
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of dilintas
Sent: Thursday, January 19, 2017 12:02 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:25941] Socket Weld WPS
The issue is that when you are checking the isometrics issued for fabrication you never find this details and especially the 2 mm gap
Sent from my Samsung Galaxy smartphone.
-------- Original message --------
From: John Henning <jhen...@deltak.com>
Date: 18/01/2017 18:44 (GMT+02:00)
Subject: RE: [MW:25933] Socket Weld WPS
Sorry to disagree –a socket weld is simply a fillet weld and a WPS can be written from a groove weld PQR to cover all fillet welds in addition to groove welds. See Table QW-452.6. Fillet welds must be referenced on the WPS and additional information for setting up the socket weld will have to appear on fabrication drawings or be included on the WPS (i.e. the 1/16 inch gap prior to performing the weld). A separate WPS for each weld configuration is not required by ASME – typically referenced to fabrication drawings.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of dilintas
Sent: Tuesday, January 17, 2017 8:43 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:25918] Socket Weld WPS
No it is not. For every configuration you should draft a specific WPS. However a WPSS for socket welds could be supported by a PQR done on button welds if all essential variables are within PQR approval range
Sent from my Samsung Galaxy smartphone.
-------- Original message --------
Date: 17/01/2017 13:00 (GMT+02:00)
Subject: Re: [MW:25914] Socket Weld WPS
Yes applicable for socket weld " fillet weld"
Ahmed Elsharkawy| QA/QC Engineer.
BV Representative Amal platform C project.
® Bureau veritas.
Mobile: (+20) 01110423873
Email: Ahmad.Sh...@gmail.com
On Jan 17, 2017 11:40 AM, "Ali Hayat" <aliha...@gmail.com> wrote:
Dear All,
Does butt weld WPS is applicable for socket weld? Can anyone provide ASME IX code reference for this ?
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0490206d-a0a5-4fdd-a513-645d5fc1eaad%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK-7o_Mz8-%2B%3DuRQm9O_%2B%3DNLDZbZZ1Zgr_T%2BZg%3Dhf1iQOr2Cbnw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/tvyiixqpkstxrtm3rh44eqym.1484664204175%40email.android.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9b1vldnqswaaeqx5rd35iebh.1484805745544%40email.android.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7A438959F2EDF14784C801E486010FE61CB6D735%40DAGN07a-e6.exg6.exghost.com.