Socket Weld WPS

640 views
Skip to first unread message

Ali Hayat

unread,
Jan 17, 2017, 4:40:33 AM1/17/17
to Materials & Welding
Dear All,

Does butt weld WPS is applicable for socket weld? Can anyone provide ASME IX code reference for this ?


Ahmad el-sharkawy

unread,
Jan 17, 2017, 6:00:39 AM1/17/17
to material...@googlegroups.com
Yes applicable for socket weld " fillet weld"

Ahmed Elsharkawy| QA/QC Engineer.

BV Representative Amal platform C project.

  ® Bureau veritas.

  Mobile:    (+20) 01110423873 

  Email:   Ahmad.Sh...@gmail.com

 

On Jan 17, 2017 11:40 AM, "Ali Hayat" <aliha...@gmail.com> wrote:
Dear All,

Does butt weld WPS is applicable for socket weld? Can anyone provide ASME IX code reference for this ?


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0490206d-a0a5-4fdd-a513-645d5fc1eaad%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

dilintas

unread,
Jan 18, 2017, 12:16:14 AM1/18/17
to material...@googlegroups.com
No it is not. For every configuration you should draft a specific WPS. However a WPSS for socket welds could be supported by a PQR done on button welds if all essential variables are within PQR approval range 



Sent from my Samsung Galaxy smartphone.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK-7o_Mz8-%2B%3DuRQm9O_%2B%3DNLDZbZZ1Zgr_T%2BZg%3Dhf1iQOr2Cbnw%40mail.gmail.com.

Unni Romes

unread,
Jan 18, 2017, 10:23:59 AM1/18/17
to Materials & Welding
If the join design is not essential variable for that particular process and all the other essential variables are within the PQR range, the WPS for butt weld will be applicable for fillet and socket weld join designs which specified in the applicable code for fabrication and erection (ie, B31.1, B31.3 etc.) 

John Henning

unread,
Jan 18, 2017, 11:44:44 AM1/18/17
to material...@googlegroups.com

Sorry to disagree –a socket weld is simply a fillet weld and a WPS can be written from a groove weld PQR to cover all fillet welds in addition to groove welds.  See Table QW-452.6.  Fillet welds must be referenced on the WPS and additional information for setting up the socket weld will have to appear on fabrication drawings or be included on the WPS (i.e. the 1/16 inch gap prior to performing the weld).  A separate WPS for each weld configuration is not required by ASME – typically referenced to fabrication drawings.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0490206d-a0a5-4fdd-a513-645d5fc1eaad%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK-7o_Mz8-%2B%3DuRQm9O_%2B%3DNLDZbZZ1Zgr_T%2BZg%3Dhf1iQOr2Cbnw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

dilintas

unread,
Jan 19, 2017, 5:52:12 AM1/19/17
to material...@googlegroups.com
The issue is that when you are checking the isometrics issued for fabrication you never find this details and  especially the 2 mm gap

dilintas

unread,
Jan 19, 2017, 5:52:13 AM1/19/17
to material...@googlegroups.com
We should not confuse between the WPS used for the PQR and a WPSS which will give direct instructions to welders on how to perform a specific weld.



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Unni Romes <unni...@gmail.com>
Date: 18/01/2017 14:14 (GMT+02:00)
To: Materials & Welding <material...@googlegroups.com>
Subject: [MW:25924] Re: Socket Weld WPS

If the join design is not essential variable for that particular process and all the other essential variables are within the PQR range, the WPS for butt weld will be applicable for fillet and socket weld join designs which specified in the applicable code for fabrication and erection (ie, B31.1, B31.3 etc.) 

On Tuesday, January 17, 2017 at 1:40:33 PM UTC+4, Ali Hayat wrote:
Dear All,

Does butt weld WPS is applicable for socket weld? Can anyone provide ASME IX code reference for this ?


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

Butch Murrell

unread,
Jan 19, 2017, 9:11:39 AM1/19/17
to material...@googlegroups.com

If they are an experienced fabricator, the 2mm gap is understood, of course that is assuming proper pipe fitting/fabricating training.  Many shop detailers of isometrics may not even know about the gap, so it doesn’t get put in the isometric drawing notes.

L.G. Murrell, Jr-“Butch”

Coastal Machine & Mechanical, LLC

Email: bmur...@coastalmandm.com

Ahmad el-sharkawy

unread,
Jan 20, 2017, 4:31:22 AM1/20/17
to material...@googlegroups.com
You can get goint preperation "fitup" from conatuction code you can find it at B31.3 for process piping and B31.1 for power piping.


Ahmed Elsharkawy| QA/QC Engineer.

BV Representative Amal platform C project.

  ® Bureau veritas.

  Mobile:    (+20) 01110423873 

  Email:   Ahmad.Sh...@gmail.com

 
On Jan 19, 2017 4:11 PM, "Butch Murrell" <bmur...@coastalmandm.com> wrote:

If they are an experienced fabricator, the 2mm gap is understood, of course that is assuming proper pipe fitting/fabricating training.  Many shop detailers of isometrics may not even know about the gap, so it doesn’t get put in the isometric drawing notes.

L.G. Murrell, Jr-“Butch”

Coastal Machine & Mechanical, LLC

Email: bmur...@coastalmandm.com

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of dilintas
Sent: Thursday, January 19, 2017 12:02 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:25941] Socket Weld WPS

 

The issue is that when you are checking the isometrics issued for fabrication you never find this details and  especially the 2 mm gap

 

 

 

Sent from my Samsung Galaxy smartphone.

 

-------- Original message --------

From: John Henning <jhen...@deltak.com>

Date: 18/01/2017 18:44 (GMT+02:00)

Subject: RE: [MW:25933] Socket Weld WPS

 

Sorry to disagree –a socket weld is simply a fillet weld and a WPS can be written from a groove weld PQR to cover all fillet welds in addition to groove welds.  See Table QW-452.6.  Fillet welds must be referenced on the WPS and additional information for setting up the socket weld will have to appear on fabrication drawings or be included on the WPS (i.e. the 1/16 inch gap prior to performing the weld).  A separate WPS for each weld configuration is not required by ASME – typically referenced to fabrication drawings.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of dilintas
Sent: Tuesday, January 17, 2017 8:43 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:25918] Socket Weld WPS

 

No it is not. For every configuration you should draft a specific WPS. However a WPSS for socket welds could be supported by a PQR done on button welds if all essential variables are within PQR approval range 

 

 

 

Sent from my Samsung Galaxy smartphone.

 

-------- Original message --------

Date: 17/01/2017 13:00 (GMT+02:00)

Subject: Re: [MW:25914] Socket Weld WPS

 

Yes applicable for socket weld " fillet weld"

Ahmed Elsharkawy| QA/QC Engineer.

BV Representative Amal platform C project.

  ® Bureau veritas.

  Mobile:    (+20) 01110423873 

  Email:   Ahmad.Sh...@gmail.com

 

On Jan 17, 2017 11:40 AM, "Ali Hayat" <aliha...@gmail.com> wrote:

Dear All,

Does butt weld WPS is applicable for socket weld? Can anyone provide ASME IX code reference for this ?


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7A438959F2EDF14784C801E486010FE61CB6D735%40DAGN07a-e6.exg6.exghost.com.
Reply all
Reply to author
Forward
0 new messages