Dear sir,

Please resolve this confusion about weld joint category.

What's the weld joint category for nozzlE  LWNRF TO SRNECK joint.

makrand sakpal

unread,
Dec 18, 2015, 10:40:09 PM12/18/15
to material...@googlegroups.com

What is the confusion?
It is Category B joint. Refer UW-3 (b).

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5672c298.8e49620a.5c2a3.453a%40mx.google.com.
For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages