Qualification

73 views
Skip to first unread message

Jayadeep C

unread,
Jun 23, 2020, 11:17:18 PM6/23/20
to Materials & Welding
If one welder qualified in CS, possible to weld SS and Low alloy


Karthik

unread,
Jun 23, 2020, 11:25:33 PM6/23/20
to Materials & Welding
Hi,
Regarding Base material qualification is OK (But please refer QW 423.1)
For Filler metal,position etc., please refer ASME Sec.IX-QW 350,351, Table QW-352 to 357 for essential variables for welder qualification and QW-360 to QW-363 for Welding Operator Qualifications.
Thanks& Regards,

 

(Karthik)

Karthikeyan.S

M: +66-892512282
E-mail : karth...@yahoo.com



On Wednesday, June 24, 2020, 10:17:15 AM GMT+7, Jayadeep C <jayadeepm...@gmail.com> wrote:


If one welder qualified in CS, possible to weld SS and Low alloy


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/39ea0722-5eda-4e38-8f5f-873032810eb4n%40googlegroups.com.

Kannayeram Gnanapandithan

unread,
Jun 24, 2020, 2:40:59 AM6/24/20
to materials-welding
Depending on process because Fno is essential. 

On Wed, 24 Jun 2020 8:47 am Jayadeep C, <jayadeepm...@gmail.com> wrote:
If one welder qualified in CS, possible to weld SS and Low alloy


harenath jha

unread,
Jun 24, 2020, 11:49:11 PM6/24/20
to material...@googlegroups.com
No not all 

On Wed, Jun 24, 2020, 08:47 Jayadeep C <jayadeepm...@gmail.com> wrote:
If one welder qualified in CS, possible to weld SS and Low alloy


Vinay Thattey

unread,
Jun 25, 2020, 11:26:33 AM6/25/20
to material...@googlegroups.com
You have to consider essential variables .