Electrode for Material SA516 Gr70

63 views
Skip to first unread message

Kiran

unread,
May 7, 2019, 8:09:14 AM5/7/19
to Materials & Welding
Dear All,

Please refer below mentioned details and please let me know, can I use this details in PWPS as per D1.1.
 
1) Material -SA 516 Gr.70 to SA 516 Gr.70

2) P No- 1 Group No - 2 to P No- 1 Group No - 2

3) F No- 4
 
4) A No-1

5) SFA No- 5.1

6) AWS No(Class) -E-6013.

I have debut about electrode.  

If any thing please wright briefly.


Thanks and Regards

Kiran 

Dinesh Somwanshi

unread,
May 7, 2019, 8:33:23 AM5/7/19
to materials-welding

Please proceed with 7018 low hydrogen electrode. Suggested h2 level should be less than 10mg.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a45e40b7-5849-44b8-80b2-9c2551ce957c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

anand gupta

unread,
May 7, 2019, 9:18:04 AM5/7/19
to material...@googlegroups.com, Kiran
I think for SA 516 GR 70 is best electrode is E7018. 

Regards 
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

ROHAN SONI

unread,
May 7, 2019, 9:26:58 AM5/7/19
to material...@googlegroups.com, Kiran
With E6013 you will not get strength you should go for E7018 electrode with low hydrogen content

Regards,

Rohan soni
8238850741

George Dilintas

unread,
May 8, 2019, 8:38:47 AM5/8/19
to material...@googlegroups.com
I would suggest E7018

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a45e40b7-5849-44b8-80b2-9c2551ce957c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Mohammed afzal Khateawdi

unread,
May 8, 2019, 8:47:12 AM5/8/19
to material...@googlegroups.com
E 7018 my suggestion...


Regards
Afzal...

Bien ND

unread,
May 9, 2019, 2:20:40 AM5/9/19
to Materials & Welding

E7016/ E7018

Vinay Thattey

unread,
May 9, 2019, 10:25:29 PM5/9/19
to material...@googlegroups.com
Dear , 6013 is a low cost b
electrode  but you will compromise on   strength of joint. The plate material selected i.e. SA 516 Gr 70 is a material of reasonable good strength . E7018 is better and appropriate choice .

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
Reply all
Reply to author
Forward
0 new messages