Hi
Set In mostly used for High pressure system it's considered mother pipe thickness only (bevel to be make only mother pipe)WPS and WQT selection to be select mother pipe.
Note if Set On Fillet weld only applicable,no need to check size and thickness.
Regards
Ramamoorthi Thangarasu
DNV- GL
--
Anandhapadmanabha pillaim
unread,
2:21 PM (2 hours ago) 2:21 PM
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
While considering the thickness, if it's a dissimilar thickness, the thickness of the smaller one and upper one should fall as per QW-451.1 if the qualification is made on a 38mm thickness coupon, the upper limit you will get unlimited still the lower one should fall within the WPS or you can combine 2 PQR and make one WPS inoder ro cover upper as well as lower limit.