Dear Experts, 

What to write the in the wps , where pulsing current ------- mentioned

iF i use SMAW process in wps pulsing current -------
iF i use GTAW process in wps pulsing current -------
iF i use SAW process in wps pulsing current -------
iF i use GMAW process in wps pulsing current -------

What to write for each procss , 

Can one one tell the answers as mentioned avove.(Applicable/not applicable/none/yes etc.)

Thanks.
Madheswaran.S

james gerald

unread,
Jul 20, 2022, 6:38:10 AM7/20/22
to material...@googlegroups.com
SMAW & SAW no Pulsing.

Only GTAW & GMAW pulsing.


It depends on your Machine capability in adjusting the below.

Peak current & Time
Background Current & Time

Upslope & Downslope

Thanks & Regards

J.Gerald Jayakumar



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/36fd9ece-5234-42e9-b1e1-fd3900b1d214n%40googlegroups.com.

james gerald

unread,
Jul 21, 2022, 7:49:25 AM7/21/22
to 'james gerald' via Materials & Welding
Though Pulsing is mentioned as a non-essential variable for GTAW, WPS is a document for Welder to follow apart from Approving. Hence necessary details shall be mentioned.

Thanks & Regards