Dear experts!


As per previous edition of ASME Sec IX, If a welder qualifies for P no. 1                                          
his range of qualification will be P1 through P11.

According to latest edition of ASME Sec IX-2010, P no. of A335 P91 material
is changed from P5B Group 2 to P15E Group 1

If a welder qualifies with P1 material, can he weld A335 P91 without additional qualification?

Regards
ASIF

WAGNER Daniel

unread,
Oct 20, 2011, 1:12:35 PM10/20/11
to material...@googlegroups.com

Dear AISF,

 

Please refer to ASME Section IX, paragraph QW-423.1:

 

Welders qualified using any P-No. 1 through P-no. 15F, P-No. 34 and P.-No. 41 through P-No. 49 are qualified for production welding of same.  Therefore, yes, he would be qualified for A335 P91 materials without further qualification.  I would however, caution that you need to ensure the welder understands the requirements of welding P15E materials and that there is a qualified procedure acceptable to product and service conditions.

 

Dan Wagner

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Vinod Kataria

unread,
Oct 21, 2011, 12:54:21 AM10/21/11
to material...@googlegroups.com

Dear All,

We have qualified procedure for Inconel 8825 P No. 45 as per ASME Section-9 with GTAW process using filler ErNiCrMo3, now we need to weld Inconel 625 P No. 43 with GTAW using the same filler i.e. ErNiCrMo3. Please suggest if we can use already qualified procedure for Inconel 825 for Inconel 625 also or we need to do the fresh qualification for this.

Thanks in advance for your kind help.

With kind regards,

Vinod Kumar Kataria

GM - Operations

Bliss Anand Private Limited,

92B/93B Sector 5

IMT Manesar,Gurgaon,

National Capital Region Delhi.

India .

Phone : +91-124-4366000 (9 Lines)

Mobile Phone : +91-9560199004

Fax : +91-124-2290884

Vinayak Kale

unread,
Oct 21, 2011, 3:07:52 AM10/21/11
to material...@googlegroups.com

You have to go for different PQR , as P No. is different , which is essential variable as per ASME IX


Regards


Vinayak Kale
OGSP - QA & I , HC - Upstream
EPC Block , 2nd Floor , Gate No.1
Saki Vihar Rd. Powai Campus
Mumbai - 400072
Ph : + 91 022 6705 3969
(M) - 9987875309
www.larsen toubro.com



"Vinod Kataria" <vinod....@blissanand.com>
Sent by: material...@googlegroups.com

10/21/2011 10:34 AM


To
<material...@googlegroups.com>
cc
Subject
RE: [MW:12735] P91 - Welder qualification


--

To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at

http://materials-welding.blogspot.com/


The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Disclaimer :This email and any files transmitted with it are intended solely for the use of the addressee(s) only and may contain confidential and/or privileged information. If you are not the addressee, then this message is not intended for you and be advised that you have received this email in error and that any use , dissemination , forwarding, printing or copying of this email is strictly prohibited. In such case please notify the sender and delete this email and any attachments with it from your system immediately.Receipt of this email by you shall not give rise to any liability on the part of Larsen & Toubro Limited

Karthik

unread,
Oct 21, 2011, 4:07:45 AM10/21/11
to material...@googlegroups.com
Hi,
Change in P.Number is an essential variable for WPS/PQR. You need to Qualify new WPS/PQR
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282

From: Vinod Kataria <vinod....@blissanand.com>
To: material...@googlegroups.com
Sent: Friday, October 21, 2011 11:54 AM
Subject: RE: [MW:12735] P91 - Welder qualification

manpreet

unread,
Oct 23, 2011, 1:50:45 AM10/23/11
to material...@googlegroups.com
Hi,

Please review QW-350 (welder qualification), change is P no. would require requalification regardless of welding process.

Regards
Manpreet Singh



From: "Vinod Kataria" <vinod....@blissanand.com>
Sent: Sat, 22 Oct 2011 16:38:25
To: <material...@googlegroups.com>
Subject: Re: [MW:12735] P91 - Welder qualification

Dear All,

We have qualified procedure for Inconel 8825 P No. 45 as per ASME Section-9 with GTAW process using filler ErNiCrMo3, now we need to weld Inconel 625 P No. 43 with GTAW using the same filler i.e. ErNiCrMo3. Please suggest if we can use already qualified procedure for Inconel 825 for Inconel 625 also or we need to do the fresh qualification for this.

Thanks in advance for your kind help.

With kind regards,

Vinod Kumar Kataria

GM - Operations

Bliss Anand Private Limited,

92B/93B Sector 5

IMT Manesar,Gurgaon,

National Capital Region Delhi.

India .

Phone : +91-124-4366000 (9 Lines)

Mobile Phone : +91-9560199004

Fax : +91-124-2290884

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.
Reply all
Reply to author
Forward
0 new messages