Dear all,

Greeting for the Day,

Which filler wire is required to weld  SS310 TO  SS316  as per code requirement.




Thanks & Regards.
Sujit Singh 

james gerald

unread,
Jun 8, 2022, 11:44:42 PM6/8/22
to material...@googlegroups.com
SS310 to SS316    use consumable ER310 or ER 309 or ER 309L

SS310 to SS316L use consumable ER 309L

Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/29f4a317-9a6a-4aa4-b705-a30b4dbd3d16n%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages