Stud Material :SA 193 GR.B7
Plate Material:IS 2062 GR.B

Dear experts,
How to qualify WPS For the stud to plate welding for the above mentioned details,as per ASME Sec IX.

Regards,
Pankaj

meisam shokri arfaei

unread,
Apr 15, 2015, 6:51:11 AM4/15/15
to material...@googlegroups.com
Please read QW-192 for tests in WPS and/or welder qualification.
Also read QW-261 for essential variables.

Regards


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a05deb5a-80a0-4859-a4f2-7180c7bd203b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer





pankaj phuse

unread,
Apr 15, 2015, 12:45:51 PM4/15/15
to material...@googlegroups.com
sir,
but qw192 is for automatic stud welding.
please guide me about the testing requirements.