welding SA-537

266 views
Skip to first unread message

zahra

unread,
Jan 2, 2014, 4:01:06 PM1/2/14
to material...@googlegroups.com
hi,would you please help me with GMAW or FCAW of SA-537 plate?it's gonna be a cylindrical shell for pressure vessel.i wanna know how to choose bevel angel?
and for GTAW of that,which electrode should i use?for 3classes?
thanks.

Octane Mac

unread,
Jan 3, 2014, 11:18:39 AM1/3/14
to material...@googlegroups.com
Attached are the suggested /preliminary welding procedures for SA-537 Cl. 1, 2 & 3. It includes consumables suggestion also for GTAW and SMAW.

Procedures have been taken from professional settings of WeldPulse Arc Edition software.

Octane


--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

SA-537 Cl. 1.pdf
SA-537 Cl. 2.pdf
SA-537 Cl. 3.pdf

zahra

unread,
Jan 3, 2014, 11:49:04 AM1/3/14
to material...@googlegroups.com
thanks a lot for that.
would you please help me with FCAW too?
i couldent choose between electrodes.

george....@gr.bureauveritas.com

unread,
Jan 7, 2014, 5:01:50 AM1/7/14
to material...@googlegroups.com

If you want to use FCAW beware of Lack of Fusion and do not use 100% CO2 as shielding gas

    best regards

    Dr. Georgios Dilintas

    Authorized Nuclear Inspector
    Authorized Inspector Supervisor
    API 510 Inspector

    I&F REGIONAL TECHNICAL MANAGER
    BUREAU VERITAS HELLAS

    Tel: +30 210 40 63 113/4
    Fax: +30 210 40 63 118
    Cell: +30 69 44 64 62 04
    (See attached file: Dilintas_George.vcf)

Inactive hide details for zahra ---03/01/2014 18:54:08---thanks a lot for that. would you please help me with FCAW too?zahra ---03/01/2014 18:54:08---thanks a lot for that. would you please help me with FCAW too?

--

To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at


http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit
https://groups.google.com/groups/opt_out.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Dilintas_George.vcf
Reply all
Reply to author
Forward
0 new messages